From: Characterization of ZnO nanoparticles grown in presence of Folic acid template
h k l | peak position |
---|---|
1 0 0 | 31.8360 |
0 0 2 | 34.5018 |
1 0 1 | 36.3329 |
1 0 2 | 47.6491 |
1 1 0 | 56.7232 |
1 0 3 | 63.0119 |
2 0 0 | 66.5315 |
1 1 2 | 68.1121 |
2 0 1 | 69.2511 |
0 0 4 | 72.7565 |
2 0 2 | 77.1527 |