Wood treatment | µg Cu/mg abraded particles | µg Cu/mL medium (eluatesa) [release in  %] |
---|---|---|
Untreated | 0.01 ± 0.02 | 0.01 ± 0.01 |
MCA-pressure treated | 2.02 ± 0.09 | 0.36 ± 0.01 [4.4%] |
CC-pressure treated | 4.26 ± 0.01 | 0.75 ± 0.01 [4.4%] |
RPMI medium (w/o wood) | na | 0.00 ± 0.01 |