Skip to main content

Table 2 Characterization of InP MUA and CdSe MUA QDs

From: Quantifying engineered nanomaterial toxicity: comparison of common cytotoxicity and gene expression measurements

Label name Total mass (g) Total moles (mol) Absorption max. (nm) Size from UV–Vis (nm) Size from DLS (nm) Zeta potential (mv)
5 nm InP MUA 0.00197 6.778 × 10−6 613 4.61 3.99 ± 0.34 − 45.8 ± 8.7
5 nm CdSe MUA 0.0094 4.899 × 10−5 617 5.43 8.84 ± 2.45 − 54.9 ± 11.6