Table 5 Tensile strength of CHI-0.1% HA fiber after 0 h, 2 h, 14 days and 28 days in the standard medium (Dulbecco’s modified Eagle’s medium).

From: Biodegradable polymer nanocomposites for ligament/tendon tissue engineering

Incubation time

Tensile strength (MPa)

0 h

213.3 ± 10.0

2 h

60.0 ± 6.7

14 days

66.7 ± 6.8

28 days

65.1 ± 6.6

  1. n = 45 in each sample (mean ± standard deviation)