Skip to main content

Table 1 Measurement results of the deposited fibers’ temperature

From: Self-powered portable melt electrospinning for in situ wound dressing

Material Spinning distance (cm) Temperature of mouse skin before e-spinning (°C) Temperature of material barrel (°C) Temperature of spinneret (°C) Temperature of dropped fibers on skin (°C)
PCL fibers 7 36–38 180–200 124–130 38.5
10 36–38 180–200 124–130 34.7
13 36–38 180–200 124–130 30.2