Table 4 Physical expansion of the multi-walled HNTs in different conditions characterized by DLS

From: Plasmonic photothermal release of docetaxel by gold nanoparticles incorporated onto halloysite nanotubes with conjugated 2D8-E3 antibodies for selective cancer therapy

Entry

Average particle size (nm)

Temperature of the colloidal solution (°C)

Experimental conditionsa

1

55

− 50

Dry ice/acetone bath, ethanol

2

72

4

Ice/salt bath, ethanol

3

110

25

Room temperature in waterb

4

134

40

White LED irradiation for 5 minc in water

5

151

50

White LED irradiation for 10 min in water

6

171

60

White LED irradiation for 15 min in water

  1. aDispersions were subjected to sonication for 5 min prior to Dynamic Light Scattering (DLS) measurements
  2. bThe DLS size distribution data for this condition are shown in Fig. 6a
  3. cHeating through the PPTT effect of AuNPs incorporated into HNTs