From: Different coatings on magnetic nanoparticles dictate their degradation kinetics in vivo for 15 months after intravenous administration in mice

Fig. 10

Ferritin and paramagnetic iron quantification over time as an indicator of MNP degradation. a Spleen and b liver ferritin concentration from 7 days after the last administration to 15 months. c Liver paramagnetic iron concentrations over time quantified from the in-phase susceptibility data. The data are shown as the means ± SD (n = 2)