SEM micrographs of the nanocoating. SEM micrographs of the nanocoating after 60 minutes of deposition from 2.5:1 of APTMS:PFTS under 22 mmHg at temperature of 40 °C (sample E). The film is 312.5 nm thick with pores in the film ranging in size between 100 - 500 nm. (a) and (b) are at magnifications 23.62 KX and 11.07 KX respectively.