Skip to main content

Table 2 Characterization of the contact asperities from AFM analysis

From: Conversion of nanoscale topographical information of cluster-assembled zirconia surfaces into mechanotransductive events promotes neuronal differentiation

 

ns-Zr15

ns-Zr25

Distance between asperities (nm)

72 ± 8

87 ± 10

Asperity diameter (nm)

43 ± 15

47 ± 17

Asperity contact area (nm2)

1954 ± 1268

2596 ± 1766