Table 1 Characterization of different molecular weight PLGA nanoparticle (NP) preparations containing PS-155 for mean size (DLS diameter), surface charge (zeta potential) and polydispersity index (PDI)

From: Investigation of PLGA nanoparticles in conjunction with nuclear localization sequence for enhanced delivery of antimiR phosphorothioates in cancer cells in vitro

PLGA polymer (50:50)

Formulations

Inherent viscosity (dL/g)

PLGA mol. wt. (kDa)

Zeta potential (mv ± SD)

Hydrodynamic diameter (DLS) (nm ± SD)

PDI

Acid terminated

NP-1

0.15–0.25

6.7–12.9

− 24.5 ± 1.2

280 ± 80

0.13 ± 0.06

NP-2

0.55–0.75

21.0–43.5

− 26.5 ± 2.0

376 ± 15

0.16 ± 0.05

Ester terminated

NP-3

0.15–0.25

6.70–12.9

− 20.2 ± 4.8

358 ± 70

0.26 ± 0.09

NP-4

0.26–0.54

12.9–21.0

− 22.4 ± 4.8

351 ± 70

0.17 ± 0.08

NP-5

0.65

43.5

− 23.3 ± 4.6

430 ± 137

0.19 ± 0.13

NP-6

0.95–1.2

73.7–91.6

− 18.3 ± 2.3

536 ± 32

0.16 ± 0.008