From: Multifunctional antibacterial bioactive nanoglass hydrogel for normal and MRSA infected wound repair

Fig. 3

Evaluation of FABA hydrogel on normal skin wound healing in mice. A Imaging of wound healing on day 0, 3, 7 and 14 after 3 M, control, FA, FAB and FABA treatment. B The wound area on day 0, 3, 7 and 14 after 3 M, control, FA, FAB and FABA treatment. C Statistics of skin wound healing rate on day 3, 7 and 14. D Statistics of skin wound closure time in different treatment groups. E Schematic diagram showed the wound area size on day 0, 3, 7 and 14. n = 6, *P < 0.05, **P < 0.01, ***P < 0.001 and n.s. means no significance