Fig. 4From: Hyaluronic acid-modified and verteporfin-loaded polylactic acid nanogels promote scarless wound healing by accelerating wound re-epithelialization and controlling scar formation A: immunofluorescence analysis of YAP expression and fibrosis biomarkers; B: Statistical analysis of YAP and TGF-βα-SMA (*: p < 0.05); C: Statistical analysis of α-SMA and MMP-3 (*: p < 0.05)Back to article page